PRODUCT DESCRIPTION
Composition: mixtures of fatty acids and their esters, hydrocarbons, waxes and inorganic carriers
Appearance: white to yellow particles
Packing: double-layer packaging in plastic bag composite woven paper bag
Net weight: 25kg/bag Safety performance: non-toxic and harmless
Storage time limit: stored in a ventilated, dry, non-corrosive warehouse for two years
PH value: 4.0-7.0
Heating loss (55℃): ≤2.0%
Inorganic content (950℃): 18.0-22.0%
APPLICABLE SCOPE
Suitable for natural rubber, synthetic rubber and reclaimed rubber.
PERFORMANCE CHARACTERISTICS
1. KT-BAH has excellent mixing effect, accelerates the dispersion of silica, carbon black and other fillers in the rubber compound, further shortens the mixing time, increases the extrusion and calendering speed, and reduces energy consumption.
2. KT-8AH makes the rubber compound have good fluidity, reduces the Mooney viscosity of the mixed rubber, improves the compactness and brightness of the extruded and calendered products, reduces the defects of the finished products, and improves the appearance quality and qualification rate of the products. .
3. KT-8AH has good plasticizing properties. It can be quickly filled with lower pressure during conversion and injection molding, and has good mold release.
4. KT-8AH has good compatibility with various rubbers. Under the premise of the recommended dosage, it has no adverse effect on the physical properties of the product, and can be widely used in various rubber ingredients.
INSTRUCTIONS FOR USE
KT-8AH can be added with other chemical compounding agents in one well during the mixing process, and the effect of adding it in advance is better.
DOSAGE RECOMMENDED
1. Add 1-4 parts of the raw rubber amount.
2. The amount of polar glue is appropriately increased.
Keyword:
KT-8AH
We could not find any corresponding parameters, please add them to the properties table
Previous

If you are interested in our products, welcome to leave us a message.

Username used for comment:
客户留言
Description:

Related Products

搜索
Search
这是描述信息

Website on mobile

这是描述信息

Wechat

这是描述信息

Whatsapp

Copyright © Qingzhou Zhongrui Industry and Trade Co., Ltd. 鲁ICP备16024654号-1 Powered by: www.300.cn seo label